--- title: "Which paint goes over previously painted wood?" description: "Clean it, key it and spot-prime bare areas — and find out first whether the existing paint is oil or water based. The ranked options, the technique that changes the " url: https://atoneplace.net/which/paint-painted-wood/ site: "At One Place" --- # Which paint goes over previously painted wood? **Which paint goes over previously painted wood?: Clean it, key it and spot-prime bare areas — and find out first whether the existing paint is oil or water based.** Adhesion failures on repainted joinery come from three causes, in order: grease, gloss and incompatibility. Kitchen and bathroom woodwork carries an invisible film of cooking grease and body oils that no amount of sanding removes, so degreasing with sugar soap or a detergent comes before abrading, not after. Gloss needs a physical key, which means abrading until the shine is gone rather than a token pass. Incompatibility is the sneaky one: modern water-based paint over old oil-based gloss can look perfect and peel off in sheets a year later, and the test is simple — rub a hidden area with methylated spirit on a rag, and if paint comes off on the rag it is water-based. Pre-1990s paintwork should be tested for lead before any sanding. ## The options, ranked *Ranked best-first for the stated job. The third column is why the others exist.* | Option | Good at | Bad at | | --- | --- | --- | | Water-based acrylic eggshell or satin | Low odour, fast recoat, keeps its colour and does not yellow in dark rooms. | Needs a bonding primer over old oil-based gloss, and it takes weeks to reach full hardness. | | Oil-based (alkyd) gloss | Flows out to a hard, wipeable film that is still the toughest option on skirting and doors. | Yellows over time, particularly out of daylight, and is slow. | | Bonding or adhesion primer | The bridge between old oil-based paint and new water-based topcoats. | An extra coat and an extra day. | | Stripping back | The only real answer where the existing paint is failing, flaking or has too many layers to detail. | Slow, and a lead hazard on older paintwork. | ## Technique that changes the outcome 1. Wash with sugar soap or detergent, rinse, and let it dry 2. Abrade with 120-180 until the whole surface is dull, then dust off 3. Spot-prime any bare wood or filler 4. Use a bonding primer if going water-based over old oil-based paint 5. Test old paintwork for lead before sanding ## What goes wrong - Sanding before degreasing, which grinds the grease into the surface - Painting over flaking or blistered paint rather than removing it - Water-based over oil-based gloss with no primer > Compiled practical guidance rather than a published standard. Product formulations vary by brand and market, so read the label — and where the work is structural, electrical or gas, the regulations that apply where you are govern rather than anything here. ## Other paint questions | For | Use | | --- | --- | | Bare wood | Knotting solution on the knots, a wood primer, then your topcoat — and prime end grain twice. | | Plastic | Any paint, provided an adhesion promoter goes on first — and on polypropylene or polyethylene, the promoter is not optional. | | Kitchens | A scrubbable acrylic eggshell or satin on the walls — and for cabinets, degrease, prime and use a proper cabinet enamel. | | Bathrooms | A moisture-resistant acrylic in a satin or eggshell sheen with a mould inhibitor — but ventilation, not paint, is the actual fix. | | Metal | Remove the rust, apply a rust-inhibiting primer the same day, then an alkyd or a direct-to-metal acrylic. | | Ceilings | A flat matt emulsion — and if there is a water stain or nicotine, seal it with a shellac-based stain block first. | | Tiles | Tile paint over an epoxy or adhesion primer on a thoroughly degreased and abraded glaze — and expect a limited life in a shower. | | Fences | A penetrating stain or fence treatment rather than a film-forming paint — and let new pressure-treated timber weather first. | | Floors | Two-pack epoxy on concrete after a moisture test and a proper grind; floor-grade varnish or floor paint on timber. | | Radiators | A radiator enamel — water-based acrylic ones no longer yellow, which ordinary gloss on a hot surface always will. | | Exterior masonry | A breathable mineral or masonry paint — and on an old solid wall, breathability matters more than any durability claim. | | Galvanised metal | A mordant wash, a self-etch primer or a purpose-made acrylic primer for galvanising — ordinary oil-based primer peels off in sheets. | | UPVC | A uPVC-specific paint or an adhesion promoter with an acrylic topcoat — and avoid dark colours, which can distort the frame. | ## Common questions ### Which paint goes over previously painted wood? Clean it, key it and spot-prime bare areas — and find out first whether the existing paint is oil or water based. ### What should I avoid? Sanding before degreasing, which grinds the grease into the surface Painting over flaking or blistered paint rather than removing it Water-based over oil-based gloss with no primer ## Related pages - [Which paint should I use on bare wood?](https://atoneplace.net/which/paint-bare-wood/) - [Which paint sticks to plastic?](https://atoneplace.net/which/paint-plastic/) - [Which paint should I use in a kitchen?](https://atoneplace.net/which/paint-kitchen/) - [Which paint should I use in a bathroom?](https://atoneplace.net/which/paint-bathroom/) - [Which paint should I use on metal?](https://atoneplace.net/which/paint-metal/) - [Which paint should I use on a ceiling?](https://atoneplace.net/which/paint-ceiling/) - [Which paint can I use on tiles?](https://atoneplace.net/which/paint-tiles/) - [Which paint should I use on a fence?](https://atoneplace.net/which/paint-fence/) - [Which paint should I use on a floor?](https://atoneplace.net/which/paint-floor/) - [Which paint should I use on radiators?](https://atoneplace.net/which/paint-radiators/) ## Sources - Typical range compiled from manufacturer specifications — At One Place (/about/)